Some questions of photogrammetric modeling of fractographic surfaces

1
Lutsk National Technical University
2
Lviv Polytechnic National University

The theoretical and experimental studies confirm the application of photogrammetric methods for studing of surfaces which is deformed by friction, tear, spoilt etc. In particular the definition of guantitative parameters of roughness surface, slope facet of broken surface, area of broken surface and etc. are given.

1. Mel'nik V.M., Sokolov V.N. i dr. Metod trehmernoj rekonstrukcii mikrorel'efa poverhnosti tverdyh tel po ih REM-stereoizobrazhenijam // Izv. RAN. Ser. fizich. 1995. E.59. №2. S.28-34. 
2. Saltykov S.A. Stereometricheskaja metallografija. M., 1970. 
3. Husu N.P., Vitenburg Ju.R., Pal'mov V.A. Sherohovatost' poverhnostej. Teoretiko-verojatnostnyj podhod. M., 1975. 
4. Chernjavskij K.S. Stereologija v metallovedenii. M., 1977. 
5. Boyde A., Ross H.F. Photo grammetry and the Scanning Electron Microscope // Photo grammetrie Record. 1975. V.8, N946. P.408-457. 
6. El-Soudani S.M. Profilometrie analysis of fractures // Metallography. 1978. 11. P.247-336.
7. Exner H., Fripan M. // Quantitative assessment o f three-dimensional roughness, anisotropy and angular distribution of fracture surfaces by stereometry // Jomal o f Microscopy. 1985. V.138. P.161-178.