Obtaining of Coumarone-Indene Resins Based on Light Fraction of Coal Tar. 3. Coumarone-Indene Resins with Methacrylic Fragments

The method for obtaining coumarone-indene resins with methacrylic fragments (CIRM) was developed with the addition of methyl methacrylate, using a light fraction of coal tar and its fraction boiling within 423–463 К. CIRM was obtained via radical cooligomerization using 2,2'-azobis (2-methyl-propionitrile) as the initiator. The effect of the initiator amount, temperature and reaction time on the yield, softening temperature and molecular weight of CIRM has been established. The structure of the synthesized CIRM has been confirmed by IR and NMR spectroscopy.