CHROME PLATING OF PRESS TOOLING USED IN THE PRODUCTION OF NEW ELASTOMERIC MATERIALS

This research has produced multicomponent titanium-doped chromium coatings to strengthen the working surfaces of press tooling dies operated under aggressive conditions during the vulcanization of products from new elastomeric materials. The pressing was carried out on a hydraulic vulcanization press 100-400 2E. with plate sizes 400x400 of new elastomeric materials based on 10 wt.% carbonized fiber from PAN (RC Helper) or (USA), which significantly increases the heat capacity of rubber based on a copolymer of vinyl develfluoride and hexopropylene by 15-30% in the operating temperature range from 323 to 348 K.  In the work, samples from mass-produced steels such as steel 20, steel 45, U8, 40H, and 40H16M were used for coating. Mixtures of powders with a dispersion of 60-250 microns of the following materials were used as reaction agents. In determining the required dispersion of reagents, we were guided by studies that found that the maximum completeness of the transformation is observed when using a reaction mixture with a fraction of 100-120 microns. The protective coatings on samples under the conditions of the SHS were obtained at the developed pilot plant DSTU12, consisting of the following main functional systems: reaction equipment; system for monitoring and controlling technological parameters; and gas utilization system. The organization of the SIS consists in creating a powder mixture and an environment that provides exothermic interaction at the local initiation of the process (ignition). Then, the reaction wave propagates spontaneously (combustion) and the synthesized product is cooled. According to the type of chemical reaction, three SWS processes can be distinguished: direct synthesis from elements; direct synthesis from compounds and exchange reactions; and metallothermal SHS (reactions with a reducing step). The surface microhardness of multicomponent chrome layers alloyed with titanium and boron is 20000 - 22000 MPa, which is due to the presence of the phase FeB. The microhardness of the alloyed Fe2В phase is 15000 – 16000 MPa. When chromium coatings are alloyed with titanium on the considered structural materials, the following phases are formed: (Fe,Cr)23C6, (Fe,Cr)7C3, Cr3C2, as well as phases: Fe2Ti,  Cr2Ti. The surface microhardness of titanium-alloyed chromium coatings is: on steel 20 – H100= 16000 MPa, (phases: (Cr,Fe)23C6, (Cr,Fe)7C3,  Fe2Ti,  Cr2Ti, α- solid solution of Ti and Cr in α- iron), on steel 45 – H100 = 18000 MPa (phases: (Cr,Fe)23C6, alloyed with titanium, α-solid solution of chromium in iron with Cr2Ti inclusions), on U8 – H100= 19500 MPa (phases: directly on the outer side of the coating there is a zone of carbides (Fe,Cr)23C6, (Fe,Cr)7C3, Cr3C2,  (Ti,Cr)C).

  1. Vasmer, E. Preparation and characterization of composites containing natural rubber, wastes rubber and cellulose nano-crystals. Master’s degree in Advanced Materials Science and Engineering. p. 94, 2022.
  2. Kozub, Y.G., Solodey, I.I. Vykorystannya MSE dlya obchyslennya termopruzhnogo stanu pnevmatychnykh shyin [Utilization of the finite element method for computing the thermoelastic state of pneumatic tires]. Opir materialiv i teoriya sporud, № 102, pp. 232–242, 2019. [in Ukrainian].
  3. Kumar, V., Alam, M.N., Manikkavel, A., Song, M., Lee, D.-J., Park, S.-S. Silicone Rubber Composites Reinforced by Carbon Nanofillers and Their Hybrids for Various Applications: A Review. Polymers. №13(14), 2021.
  4. Nesterenko, S. V., Troshin, V. M., Bannikov, L. P., & Karchakova, V. V. Improving the corrosion resistance of steel and alloys in coal-tar processing. Coke and Chemistry, № 59(10), pp. 389–395, 2016.
  5. Sereda, B.P., Baskevych, O.S., Kruhliak, I.V., Sereda, D.B., Kruhliak, D.O. Otrymannia zakhysnykh pokryttiv z vykorystanniam kompleksnykh funktsionalno aktyvnykh shykht ta elektroosadzhenniam [Obtaining protective coatings using complex functionally active layers and electrodeposition]. Kamianske: DDTU. 2023. 191 p. [in Ukrainian].
  6. Cheshko, F. Microscopic Study of the Coal Tar Carbonaceous Dispersed Phase. Chemistry & Chemical Technology, №5(3), pp. 355-362, 2011.
  7. Varma, A., Rogachev, A.S., Mukasyan, A.S., Hwang, S. Combustion synthesis of advanced materials: Principles and applications. In Advances in Chemical Engineering. J. Wei (Ed.), New York: Academic Press, №. 24. pp. 79–226, 1998.
  8. Kirdyashkin, A.I., Salamatov, V.G., Maksimov, Y.M., Sosnin, E.A., Tarasenko, V.F., Gabbasov, R.M. Osobennosti spektra opticheskogo izlucheniya v protsessakh goreniya s obrazovaniem kondensirovannykh produktov goreniya [Features of the spectrum of optical radiation in combustion processes with the formation of condensed combustion products]. Combustion, Explosion, and Shock Waves, Vol. 46, №1, pp. 132–135, 2010. [in Ukrainian].
  9. Sereda, D., Sereda, B. High-performance chrome coatings to protect against wear and corrosion. Steel Properties and Applications in Conjunction with Materials Science and Technology, pp. 39–41, 2021
  10. Konovalenko, A.D., Dragobetsky, V.V. Novyye napravleniya razvitiya SVS–tekhnologiy [New trends in SHS technologies]. Sistemnyye tekhnologii, № 6, pp. 68–73, 2003. [in Ukrainian].
  11. Antypenko, A.M., Byelas, O.M., Voytov, V.A., Votchenko, O.S. Osnovy tribologiyi [Fundamentals of Tribology]. Kharkiv: KhNTUSG, 2008. [in Ukrainian].