circulation rate

Peculiarities of Producing an Electrolytic Iron Powder from Rolling Manufacture Waste

The electrolytic iron powder with controlled shape and size of particles and required structural, physical and functional properties was synthesized. The electrolytic precipitation of dispersed iron was carried out using a steel soluble anode and a titanium cathode. Sulfate electrolyte was used; the shape of the cathode was a plate; the electrolysis time was 1 h. Experimental studies were carried out using correlation-regression analysis. The average particle size and morphology were determined using optical microscopy.