мікроструктура

Вплив карбонатних добавок на властивості портландцементу композиційного

The effect of carbonate additives on physical and mechanical properties of type II Portland cement was investigated. It was shown that calcium carbonate which is added as fine ground mineral additive, participates in the phase composition and microstructure formation of Portland composite cement paste.

Multimodal composite Portland cements, modified with ultrafine mineral additives

The principles of creating of multimodal composite Portland cements with optimized void filling, that based on synergistic combination of ultrafine active mineral additives with superplasticizer were established. The optimization of multimodal multicompositе Portland cements was carried out and the relationship between the phase composition, microstructure and strength of the cement matrix were investigated.

The research of a phase composition and a microstructure of hydrated cement by mechanoactivated bonding substance with an additive of microsilica

The physico-chemical methods of the research of hydrated cement by mechanoactivated bonding substance with organo-mineral additive (microsilica + C-3) was presented. It was explored the influence of the additive into the kinetics of formation lowly basic calcium hydrosilicate.

Дослідження сухих будівельних сумішей для промислових підлог

In this paper prescriptions of dry building mixes for industrial floors were developed. Main indicators for such material are enough spreadability of fresh mixture during certain period of time, needed for its enclosing, high early strength, minimal deformation of hardened material. Technology of industrial floors construction in buildings with high loading is showed. Investigation of quartz sand with different granulometry on physical and mechanical properties of dry building mix for industrial floors is conducted.

Модифіковані оздоблювальні розчини з добавкою каоліну

Finishing mortars for decorative and protective facade coatings where natural kaolin is a major component were developed. The chemical and phase composition and microstructure of kaolin were investigated. Ultrafine kaolin (SSA = 1,58 m2/g) actively participates in the formation of phase composition and microstructure of the cement matrix of finishing mortars. Nanoscale systems of clay minerals due to plasticizing effect and filling influence provide improved adhesion-cohesive properties of finishing mortars.

The Use of Granulated Modofoed Lime for Expansive Cement with High-Energy Self-Tension

The article examines the features of hardening and structurization processes of cement with high-energy self-tension. The physical-chemical methods of the research confirm that the use of the granulated expanding additive leads not only to an increase in expansion but also proves to form zones with different hydrated phases around granule

Мікроструктура стоматологічного литого сплаву Родент на основі Ni-Cr-Mo

Досліджено мікроструктуру стоматологічного сплаву Родент на основі Ni-Cr-Mo після лиття у вакуум-печі. За допомогою методу енергодисперсійної спектроскопії проведено хімічний аналіз, а за допомогою дифракції зворотньо відображених електронів в растровому електронному мікроскопі проведено топографію кристалографічної орієнтації. Встановлено, що після лиття мікроструктура містить дендрити твердого розчину, що зміцнють нікель-хром матрицю (γ-фазу). Показано, що всередині дендритів спостерігаються виділення карбідів молібдену, евтектика γ-P і декілька частинок оксиду алюмінію.

Вплив оксидів заліза на властивості безфлуористих емалевих склофрит та покриттів

Досліджено вплив оксидів заліза на властивості безфлуористих емалевих склофрит та покриттів в системі Na2O– B2O3– SiO2. Встановлено, що введення додатку Fe2O3 у кількості 0,4 мол.% замість SiO2 в безфлуористій склоемалі покращує оптико-колірні характеристики покриттів, забарвлених червоним селенокадмієвим пігментом.