Using light fraction of coal tar (5.75 wt % of coumarone and 44.45 wt % of indene), glycidyl methacrylate and styrene, the coumarone-indene resin with epoxy groups (CIRE) has been synthesized. Monoperoxy derivative of diglycidyl ether Bisphenol A (PO) was used as an initiator. The possible formation of CIRE has been studied on the model systems consisting of PO, glycidyl methacrylate, indene or coumarone, or styrene, or mixture of mentioned compounds. The synthesized product has been investigated as a polymer additive to bitumen-polymer blends (BPB). The effect of CIRE amount, temperature and time on the BPB operational characteristics has been examined. By means of IR-spectroscopy the structures of CIRE, bitumen and BPB were determined.
[1] McNally T. (Ed.): Polymer Modified Bitumen. Properties and Characterization. Woodhead Publ., 2011.
[2] Fang C., Li T., Zhang Z., Jing D.: Polym. Composite, 2008, 29, 500. https://doi.org/10.1002/pc.20390
[3] Pyshyev S., Gunka V., Grytsenko Y., Bratychak M.: Chem. Chem. Technol., 2016, 10, 631. https://doi.org/10.23939/chcht10.04si.631
[4] Bratychak M., Grynyshyn O., Astakhova O. et al.: Ecolog. Chem. Eng. S, 2010, 17, 309.
[5] Bratychak M., Chervinskyy T., Astakhova O. et al.: Chem. Chem. Technol., 2010, 4, 325.
[6] Strap G., Astakhova O., Lazorko O. et al.: Chem. Chem. Technol., 2013, 7, 279. https://doi.org/10.23939/chcht07.03.279
[7] Ivashkiv O., Astakhova O., Shyshchak O. et al.: Chem. Chem. Technol., 2015, 9, 69. https://doi.org/10.23939/chcht09.01.069
[8] Bratychak M., Iatsyshyn O., Shyshchak O. et al.: Chem. Chem. Technol., 2017, 11, 49. https://doi.org/10.23939/chcht11.01.049
[9] Bratychak M., Ripak O., Namiesnik J. et al.: Chem. Chem. Technol., 2018, 12, 93. https://doi.org/10.23939/chcht12.01.093
[10] https://www.chemicalbook.com/ChemicalProductProperty_EN_CB3415111.htm
[11] Bazyliak L., Bratychak M., Brostow W.: Mater. Res. Innovat., 1999, 3, 132. https://doi.org/10.1007/s100190050138
[12] Braun D., Cherdron H., Rehahn M. et al.: Polymer Synthesis: Theory and Practice. Springer-Verlag, Berlin Heidelberg 2013. https://doi.org/10.1007/b138247
[13] BS EN 13589:2008. European Standard. Bitumen and bituminous binders. Determination of the tensile properties of modified bitumen by the force ductility method
[14] BS EN 1426:2000. European Standard. Bitumen and bituminous binders. Methods of tests for petroleum and its products. Determination of needle penetration
[15] BS EN 1427:2007. European Standard. Bitumen and bituminous binders. Determination of the softening point. Ring and Ball method
[16] BS EN 13614:2011. European Standard. Bitumen and bituminous binders. Determination of adhesivity of bituminous emulsions by water immersion test
[17] Gagin M., Bratychak M., Shyshchak O., Waclawek W.: Chemia i Inzyneria Ekologiczna, 2004, 11, 27.
[18] Bratychak M., Astakhova O., Shyshchak O. et al.: Chem. Chem. Technol., 2017, 11, 509. https://doi.org/10.23939/chcht11.04.509